  现在很多消费者别墅铜大门的使用很长一段时间或多或少会出现一些锈铜或铜现货,很多消费者在遇到这样的问题不知道如何去做,然后山东铜门制造商介绍你更多这样的问题应该如何处理。  
  Now many consumers will have some rusty copper or copper in stock for a long time. Many consumers don't know how to do it when they encounter such problems. Then Shandong copper door manufacturer introduces you how to deal with more such problems.  
 加热方法。该方法主要用于浅层锈的腐蚀。生锈的主要成分是FeO说,它的分子结构是相对宽松的,所以使用热扩张和冷收缩的原则可以使铁生锈的一部分。但是,当使用这种方法,必须注意添加接收容器(如锅和其它金属容器),除了更好添加一些水。其次是加热时间要控制,一般高温几分钟后,拿出打湿毛巾盖住,铁锈会自然脱落。选择加热除锈的方法,对象应该是高质量的铁锈比较浅,不能被严重腐蚀,而且铜体已经非常脆弱,用加热的方法除锈,否则铜制品的严重腐蚀将无法承受高温和破碎。   
山东铜门
Heating method. This method is mainly used for shallow rust corrosion. The main component of rust is FeO, which says its molecular structure is relatively loose, so using the principles of thermal expansion and cold shrinkage can make iron rust part of it. However, when using this method, care must be taken to add receiving containers (such as pots and other metal containers), except that it is better to add some water. Secondly, the heating time should be controlled. Generally, after a few minutes of high temperature, take out a wet towel to cover it, and the rust will fall off naturally. If we choose the method of heating to remove rust, the object should be high-quality rust which is shallow and can not be seriously corroded. Moreover, the copper body is very fragile. If we use the method of heating to remove rust, the copper products will not be able to withstand the high temperature and crushing.
  干刷的方法。铜制品上的铜锈斑或锈斑附着较少,应尽量避免使用酸性液体等化学手段,但可采用干刷法。具体方法是选择大小合适的油刷,将棕色头发的顶端刷短0.5-0.7厘米即可。将锈迹斑斑的待刷铜片放在玻璃板上,固定好,握住油刷根部,刷匀,注意用力,否则效果不好,然后用清水冲洗干净即可。
  Dry brush method. Copper rust spots or rust spots on copper products are less attached, so chemical means such as acid liquid should be avoided as far as possible, but dry brush method can be used. The specific method is to choose the right size of oil brush, and shorten the top brush of brown hair to 0.5-0.7cm. First, place the rusty copper to be brushed on the glass plate, fix it, hold the root of the oil brush, brush evenly, pay attention to the force, otherwise the effect is not good, and then wash it with water.